Inconel® Alloy 625 is a corrosion resistant nickel-chromium-molybdenum alloy. It is doped with niobium, which interacts with the molybdenum to provide high strength without additional heat treatment.
Zusammensetzung | UNS N06002 % |
Nickel | 58 min |
Molybdän | 8.00 - 10.00 |
Schwefel | 0.015 max |
Silizium | 0,50 max |
Chrom | 20.00 - 30.00 |
Niobium + Cobalt | 3.15 - 4.15 |
Titan | 0.4 max |
Aluminium | 0.4 max |
Eisen | 5 max |
Mangan | 0.5 max |
Kohlenstoff | 0,10 max |
Phosphor | 0.15 max |
Metrisch | Englisch | |
Dichte | 8.44 g/cm³ | 0.305 lbs/in³ |
Electrical resistivity | 1.29 µohms/m | 776 µohms/ft |
Thermal conductivity | 9.8 W/m-K | 68 Btu-in/ft²hr-°F |
Cold worked % | Yield strength | Ultimate tensile strength | Elongation % |
0 | 820 MPa [119 ksi] | 1165 MPa [169 ksi] | 36 |
20 | 1200 MPa [174 ksi] | 1496 MPa [217 ksi] | 6.1 |
37 | 1407 MPa [204 ksi] | 1751 MPa [254 ksi] | 3.3 |
50 | 1600 MPa [232 ksi] | 1889 MPa [274 ksi] | 3.2 |
60 | 1737 MPa [252 ksi] | 1993 MPa [289 ksi] | 3.1 |
68 | 1820 MPa [264 ksi] | 2055 MPa [298 ksi] | 2.1 |
75 | 1924 MPa [279 ksi] | 2144 MPa [311 ksi] | 2.3 |
All data represent results from a 25.4 cm [10 in] test gauge length. Values are typical and may not represent all diameters. Test method will affect results.